Proposed development- Printing with easy to mix Titanium alloys on Mendel printer
Samples metal parts from paste:
Extruder: can be used ParametricSyringeExtruder
Solidification: vacuum chamber, heat - from 100C - 820C step +5C/min, 25min under 820C, then holding vacuum, drop temperature to 350C, and release vacuum valve.