For my final examination, I would like to analyze the PETG filament.I print Single-walled components(0.5 mm) with the Slic3r. In the pictures you see the first 3 layer and the settings.

In the second layer is a problem when the speed is increased.

Has anyone experience with single-walled components? Does anyone have tips for settings?

Thanks for you help in my current situation.
tongue sticking out smiley
Attachments:
open | download - first layer.jpg (74.5 KB)
open | download - second layer.jpg (85.8 KB)
open | download - third layer.jpg (93.6 KB)
open | download - speed settings.jpg (65.8 KB)
open | download - temperature settings.jpg (43.6 KB)
Re: Problems with the first layers confused smiley
July 05, 2017 12:47PM
PETG recommended temperature is between 240 and 260.
Re: Problems with the first layers confused smiley
July 05, 2017 05:34PM
nozzle too high
Re: Problems with the first layers confused smiley
July 06, 2017 05:20AM
1st layer too fast, try setting it at 15mm/s