I'm getting close to having all issues ironed out. The one I can't resolve is inconsistencies in the way layers are being laid down. I'm using PETG. My hotend is 260C based on manufactures recommendation and some tinkering. The bed is at 75C. I fine tuned my E steps and other calibrations based on Triffid Hunter's calibration guide. The X and Y belts are pretty tight. The X axis is level. The bed is level. I'm using .2mm layer height and .5mm layer width, which was calibrated.. The acceleration was set at 1400 based on the P3 Steel firmware I used. I changed that to 1000, and that is what you are seeing in this picture. It still happens. I'm not sure what else to do and would love some guidance. What can I do to get these to lay evenly?