My skeinforge (40) profile was doing too much retraction too fast and it was causing jams in my extruder so I started from scratch. But now the printer move really really slowing from home to where the print begins. I can't get a good first layer because all the plastic in the nozzle drips out on the way to start printing. Anyone know why it's doing this? It seems like it must be default behavior but why on earth would anyone want this?
Edited 1 time(s). Last edit at 07/13/2011 03:14PM by unicoder.