Quote
the_digital_dentist
What are the first and second layer thicknesses? Does the hot-end temperature remain steady?
Looking at the values, I think that this might be a good start.
The first layer is set to 0.35mm (nozzle size) this I believe should be around 0.28mm instead.
The other layers are 0.25mm
The nozzle temp is 195 at the first layer and drops to 190 on all the other layers.
Did have good results using this in the past