So far, I've printed pretty much one thing at a time, and so far, my prints have pretty much all come out decent. Maybe not 100% perfect, but definitely functional.
But today, I had my first print snarl-up. I was trying to print
this (nine of them at once on the plate), the way the author printed them (upside down), and after the first handful of layers were down and looking good, I left it be and ate dinner and put my daughter to bed. When I came back to it, it was a snarled up mess glued to the nozzle.
I then printed one by itself, and that printed fine, although it was a bit small for the magnets I have, so I scaled it up and printed again. I did a handful of test prints, and in doing so while watching it, I found that it lays down the first layer fine, it continues to lay everything down fine until some point after it gets to the top of the shaft and starts to expand out. I noticed that at some point after it does that, the outer wall appears to 'curl up' to where it ends up at last .5mm higher than the bottom of the nozzle. I suspect that's why when printing the nine of them, it snarled up - as long as I'm only printing the one, the nozzle stays within the bounds of this 'lip' and it never causes issues. It seems like it doesn't complete cooling right away since as the nozzle moves around it, the material pushes out slightly. When printing one, it works itself out and by the end, it prints fine, but when printing the nine of them, I suspect enough time passed from one to the next to allow the material to cool and cease to be pliable, and the print head then knocked them over one by one and sent the whole print sideways.
I've tried slowing the print down and reducing the flow (Although the display on the printer doesn't seem to reflect the reduced flow rate specified by Cura on the LCD), but nothing seems to change it.
Any ideas why, seemingly only when the print starts to increase in width, it starts to create this 'lip' that essentially ends up straightening itself out by the end?