As I promised... I can show you the same material after drying. Amazing result. I dried it in kitchen oven like this (150C during 4 hours): I use capton on heated bed (104-110C) BUT it should be clean. Print at the same place second time if it doesn't stick first time - it works. Or you can clean capton sufarce from fat and dust. BR, Sergeyby SergeyA - General
I tried different materials and bed temperature (glass fiber, 3M blue tape, capton). I don't have access to Garolit yet. Blue tape comes off the bed together with printed part, fiber glass keep Nylow while hot after printing and left material after short timeI). I found that Nyton stick good enough on capton, but not always. It looks like it stisks good at 110C bed temperature and more. I am inveby SergeyA - General
Hi All, SelfMade for RepMan 3.1DH. Bit less than you discuss, but it works fine. 270*220mm. Unfortunately thickness of cupper is little bit various through the surface. Resistance is about 1.1Ohm - I expected bit less. Finally it looks like Printing ABS, bed temperature ~108C (lack of copper thickness variations) Any questions? BR, SergeyA P.S. Sorry for Russian notes there. Photos are noteby SergeyA - New Zealand RepRap User Group