I have the mk1 heat bed I calibrated it 8 points in the corners left right front to back but for whatever reason it seems to sink in the middle ever so slightly. Do I need to make some form of a brace? Is this maybe warped during central pressure during a heat cycle?
Re: heat bed warp?
March 12, 2013 06:04PM
You have to put something flat on top of it like glass to print on. For ABS, put PET tape on top of the glass and heat to 110 C or so. For PLA, you can print directly on glass heated to 60C or so. There are coating people use to improve adheasion like hair spray or PVA glue for PLA.
Re: heat bed warp?
March 12, 2013 06:08PM
I have glass on it that is the odd part I guess I need to see about getting a new piece of glass maybe this one is warped
Re: heat bed warp?
March 12, 2013 06:36PM
How thick is the glass? I use 3 mm.
Re: heat bed warp?
March 12, 2013 06:58PM
I believe this is about the same its just traditional plate glass for windows
Re: heat bed warp?
March 12, 2013 07:12PM
What's known as "single strength" glass should be fine. In the USA, it's 3/32" thick.
Re: heat bed warp?
March 12, 2013 07:19PM
How much of a variation are you seeing?