That's call plain old physics. Hot air trapped in the part as its cool down will create enough vacuum to suck in the still warm plastic.
It happens also with PLA but due to lower temperatures it's effects are minimum.
To solve the problem you need either to increase the number of perimeters and top layers or keep a surce of heat close to the part so the cooling takes more time.