Hello
My current issue is that when heating the tip prior to print, there is excessive runoff from the nozzle. Not a huge issue to wipe clean, but when I start to print, the first few segments do no have enough PLA material to make a line and just form sticky dots. I have combated this by creating a nice thick 3-pass skirt. Is there another way to fix this?
Blue PLA @ 180 (relatively accurate thermistor)
Mix shop nozzle w additional passive cooling
spinter
slic3r 9 (which settings would you like to know about?)
pronterface
blue tape room temp
Regards