It's been a long time since I had to ask a question here...
I've tried other PLA and usually got it to stick to my Heated Kapton bed at the right temprature.
However, I am having trouble finding the right temp for this MG Chemicals Red PLA.
I have tried 60-95, 40, 0. Zero almost worked. It still lifted around the edges.
Could it be I'm printing too hot? 210-220 (sugested)
50% White glue/water on the Kapton or just using blue tape work, but leave a mat finish. I would prefer the gloss of the glass or Kapton.
I only tried once on raw glass. Will have to try again.
Anyone using MG PLA please help.
Thanks,