Re: New print surface material? November 03, 2015 09:57AM |
Registered: 11 years ago Posts: 25 |
Re: New print surface material? November 03, 2015 10:04AM |
Registered: 10 years ago Posts: 517 |
Re: New print surface material? November 03, 2015 10:10AM |
Registered: 10 years ago Posts: 1,699 |
Re: New print surface material? November 03, 2015 12:58PM |
Registered: 13 years ago Posts: 153 |
Re: New print surface material? November 03, 2015 01:42PM |
Registered: 11 years ago Posts: 25 |
Re: New print surface material? November 03, 2015 01:57PM |
Registered: 10 years ago Posts: 517 |
Re: New print surface material? November 03, 2015 02:18PM |
Registered: 13 years ago Posts: 153 |
Re: New print surface material? November 03, 2015 05:58PM |
Registered: 9 years ago Posts: 77 |
Re: New print surface material? November 03, 2015 07:00PM |
Registered: 11 years ago Posts: 140 |
Quote
Phytone
Sometimes I think we over complicate the matter.
Mine is stuck down with tape that cost 50p for 10metres and is 3 years old. I have no idea what it is made from, and nor do I care.
It holds the printbite fast at 65 deg, which is my optimum temp for PLA - has been on for a while and no evidence it needs replacing.
Re: New print surface material? November 05, 2015 01:30AM |
Registered: 17 years ago Posts: 80 |
Re: New print surface material? November 05, 2015 02:03AM |
Registered: 10 years ago Posts: 1,699 |
Re: New print surface material? November 05, 2015 02:10AM |
Registered: 11 years ago Posts: 169 |
Quote
John Meacham
Out of curiosity, has anyone tried UV curing glue to hold their print surface to glass?
The glue is generally good to 180C so should be okay at printbed temperatures. It would be very easy to apply because you can spend all the time you want squeezing the air bubbles out and getting things aligned since it is a liquid before zapping it.
I ordered some cheap no name UV glue and will try it with my PEI/glass printbed.
If the cheap glue doesn't hold up well at temperature but seems promising otherwise then I will buy the expensive 3M stuff that is officially rated at 180C.
A random demo of UV curing glue, [www.youtube.com]
I think chemically it is similar to super glue (cyanoacrylate) except the polymerization is triggered by UV light rather than moisture.
Re: New print surface material? November 05, 2015 11:52AM |
Registered: 17 years ago Posts: 80 |
Quote
simspeed
Quote
John Meacham
Out of curiosity, has anyone tried UV curing glue to hold their print surface to glass?
The glue is generally good to 180C so should be okay at printbed temperatures. It would be very easy to apply because you can spend all the time you want squeezing the air bubbles out and getting things aligned since it is a liquid before zapping it.
I ordered some cheap no name UV glue and will try it with my PEI/glass printbed.
If the cheap glue doesn't hold up well at temperature but seems promising otherwise then I will buy the expensive 3M stuff that is officially rated at 180C.
A random demo of UV curing glue, [www.youtube.com]
I think chemically it is similar to super glue (cyanoacrylate) except the polymerization is triggered by UV light rather than moisture.
Will the UV light penetrate the PrintBite? Is line of sight for the rays necessary to cure? If it is...how do you get the UV to the glue between two opaque sheets?
Re: New print surface material? November 05, 2015 02:08PM |
Registered: 10 years ago Posts: 483 |
Re: New print surface material? November 05, 2015 03:12PM |
Registered: 9 years ago Posts: 126 |
Re: New print surface material? November 06, 2015 02:53AM |
Registered: 10 years ago Posts: 1,699 |
Quote
DaveOB
Took me 3 or 4 prints of a first layer to get the height correct. I have Auto Bed Leveling using a manual endstop switch, so was able to very easily adjust the nozzle height by 0.01 each time in the starting gCode.
Re: New print surface material? November 07, 2015 03:07PM |
Registered: 9 years ago Posts: 126 |
Re: New print surface material? November 07, 2015 03:59PM |
Registered: 10 years ago Posts: 1,699 |
Quote
DaveOB
and only release after bed cools to below 80C.
Re: New print surface material? November 07, 2015 04:12PM |
Registered: 9 years ago Posts: 126 |
Quote
Treito
Quote
DaveOB
and only release after bed cools to below 80C.
Hi Dave,
Many thanks for the answer. That is why I ordered to pieces for each printer so I can exchange the surface after a print. Unfortunately your design cannot be convert for my printers but for my Ormerod 2 I have an idea or more than one but this will be too off-topic.
I am afraid that I will not get my Printbites before Wednesday in the evening because the parcel was not transported today (other companies do transport even on Saturdays) and as I am probably not at home on Monday I can make a date for catching up the parcel at the depot not for Wednesday. Luckily the depot is nearby my work So I have an extra travel of about 200 metres by car.
Best regards,
Sven
Re: New print surface material? November 08, 2015 03:28AM |
Registered: 10 years ago Posts: 1,699 |
Re: New print surface material? November 08, 2015 03:33AM |
Registered: 9 years ago Posts: 126 |
Re: New print surface material? November 08, 2015 03:59AM |
Registered: 10 years ago Posts: 1,699 |
Re: New print surface material? November 12, 2015 03:46AM |
Registered: 10 years ago Posts: 1,699 |
Re: New print surface material? November 15, 2015 10:53AM |
Registered: 10 years ago Posts: 425 |
Re: New print surface material? November 15, 2015 11:46AM |
Registered: 10 years ago Posts: 1,699 |
Re: New print surface material? November 15, 2015 12:04PM |
Registered: 10 years ago Posts: 425 |
Re: New print surface material? November 15, 2015 12:13PM |
Registered: 10 years ago Posts: 1,699 |
Re: New print surface material? November 15, 2015 12:21PM |
Registered: 10 years ago Posts: 425 |
Re: New print surface material? November 15, 2015 12:31PM |
Registered: 10 years ago Posts: 1,699 |
Re: New print surface material? November 15, 2015 12:38PM |
Registered: 10 years ago Posts: 517 |
Quote
Mutley3D
avoid ispropyl alcohol as this can leave a film on the surface.